Abstract
Transparent TiO
2 single layer and TiO
2/Ag/TiO
2(TAT) tri-layer films were deposited by DC and RF magnetron sputter on a polyimide substrate at room temperature. During the TAT deposition, the thickness of the TiO
2 layer was kept at 20 nm, while the Ag interlayer was varied as 10, 15, 20 nm to.....